430

Ferritic Stainless Steel

ASTM Designation

EN Designation

430

1.4016

S43000

X6Cr17

 

501 is the base alloy in the ferritic group. It exhibits good resistance in corrosive environments or atmospheric exposures, as well as sulphurous gases. It is ductile in annealed condition and can be formed by rolling, folding or drawing operations. It is not excessively hardened during cold working.

 

C

Si

Mn

P

S

Cr

Ni

≤ 0.120

≤ 1.00

≤ 1.00

≤ 0.040

≤ 0.030

16.00-18.00

≤ 0.75

 

UTS

65 ksimin

0.2% YS

30 ksi min

Elongation

22% min

Hardness

max 89 HRB