Grade
347H
347H has increased resistance to intergranular corrosion and is useful in strongly oxidizing environments due to the addition of niobium (formerly columbium). Products are supplied to meet ASTM, ASME, NACE, UNS and EN standards where appropriate. UNS S34709.
Mechanical Properties* (In Annealed Condition)
Properties |
Unit of Measure |
347H |
Tensile Strength |
ksi |
75 min |
0.2% Yield Strength |
ksi |
30 min |
Elongation |
% |
40 min |
Hardness |
HV |
92 max |
*Nominal room temperature mechanical properties. Typical data. Not suitable for design or specifications
Composition
Element |
|
347H |
Cr |
Chromium |
17.0-19.0 |
Ni |
Nickel |
9.0-13.0 |
Mn |
Manganese |
2.000 max |
Si |
Silicon |
0.750 max |
P |
Phosphorus |
0.045 max |
C |
Carbon |
0.04-0.08 |
S |
Sulfur |
0.030 max |
Nb + Ta |
Niobium + Tantalum |
Min 10XC, max 1.0 |
Fe |
Iron |
Balance |
FEEL FREE TO CONTACT US
Address: 104G, Building 1, No. 196 Yangtai Road, Baoshan District, Shanghai
Follow Us


Whatsapp Elsa
Copyright © 2024 Shanghai Boxu International Trade Co., Ltd.
Powered by www.300.cn SEO Privacy Policy